Abstract
In case of the slender mass concrete like attached wall, retaining wall and bridge tower, the low heat cement and the control joint are mainly used for thermal cracking control. However, even if these cracking control methods are considered, it is impossible to control thermal cracks perfectly, because the external restraint is largely in these mass concrete. Because these cracks occurring in slender mass concrete members almost penetrate concrete member, the special cracking control is demanded in these mass concretes. The vertical pipe cooling method improving existing pipe cooling method was developed for the active thermal cracking control of slender mass concrete, and applied at the field attached wall. In results, the maximum temperature dropped more than $10^{\circ}C$ by vertical pipe cooling method, and the cracks decreased about more than 50%.
합벽, 옹벽, 교량 주탑과 같이 세장한 매스콘크리트 구조물의 경우 온도균열 제어를 위해 저발열 콘크리트 배합의 적용 및 균열유발줄눈의 설치 등이 주로 적용되고 있다. 하지만 이러한 대책이 적용되어도 세장한 매스 구조물들은 내부구속에 비해 외부구속이 크기 때문에 완벽한 균열제어가 불가능하고, 특히 균열이 발생하게 되면 거의 관통을 하기 때문에 온도균열제어를 위한 특별한 관리가 필요하다. 합벽, 옹벽, 교량 주탑과 같이 세장한 매스콘크리트 구조물의 적극적인 온도균열 제어를 위하여 기존의 파이프쿨링 공법을 개선시킨 연직파이프쿨링 공법을 개발하였으며, 현장 우수조/중수조 합벽 콘크리트에 적용이 되었다. 그 결과 합벽의 중심부 최고 온도를 10도 이상 낮츨 수 있는 것으로 나타났으며, 균열은 50% 이상 감소시킬 수 있는 것으로 나타났다.