Abstract

Purpose: This study was to assess the effect of surface and heat treatment on the bond strength of veneering ceramics to zirconia. Methods: The specimens were divided into 7 groups according to surface treatment and heat treatment conditions prior to porcelain application. ten specimens from each group were subjected to a 3-point flexural test. In addition the influence of surface and heat treatment on surface roughness values and phase transformation of zirconia was evaluated. Statistical analysis was performed with one-way ANOVA and post hoc Tukey's test. Results: Bond strength ranged from $20.67{\pm}3.13MPa$ to $32.69{\pm}4.52$. Bond strength of surface treatment group was lower than that of control group but only $Al_2O_3$ sandblasting group was significant difference. Bond strength of heat treatment group was higher than that of surface treatment group but there was no statistical significance. Conclusion: Bond strength of veneering ceramics to zirconia was affected by surface and heat treatment.

Keywords

References

  1. De Jager N, Pallav P, Feilzer AJ. The influence of design parameters on the FEA-determined stress distribution in CAD-CAM produced all-ceramic crowns. Dent Mater, 21, 242-251, 2005. https://doi.org/10.1016/j.dental.2004.03.013
  2. Fischer J, Stawarczyk B. Compatibility of machined Ce-TZP/$Al_{2}O_{3}$ nanocomposite and a veneering ceramic. Dent Mater, 23, 1500-1505, 2007. https://doi.org/10.1016/j.dental.2007.01.005
  3. Garvie RC, Nicholson PS. Phase analysis in zirconia systems. J Am Ceram Soc, 55, 303-305, 1972. https://doi.org/10.1111/j.1151-2916.1972.tb11290.x
  4. Guazzato M, Quach L, Albakry M, Swain M V. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent, 33, 9-18, 2005. https://doi.org/10.1016/j.jdent.2004.07.001
  5. International Organization Standardization. Metalceramic dental restorative systems: ISO 9693. ISO, 1999.
  6. Isgro G, Pallav P, van der Zel JM, Feilzer AJ. The influence of the veneering porcelain and different surface treatments on the biaxial flexure strength of a heat-pressed ceramic. J Prosthet Dent, 90, 465-473, 2003. https://doi.org/10.1016/j.prosdent.2003.08.003
  7. Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater, 14, 64-71, 1998. https://doi.org/10.1016/S0109-5641(98)00011-6
  8. Kim ST, Cho HJ, Lee YK, Choi SH, Moon HS. Bond strength of Y-TZP-zirconia ceramics subjected various surface roughening methods and layering porcelain. Surf Interface Anal, 42, 576-580, 2010. https://doi.org/10.1002/sia.3209
  9. Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater, 15, 426-433, 1999. https://doi.org/10.1016/S0109-5641(99)00070-6
  10. Luthy H, Loeffel O, Hammerle CHF. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater, 22, 195-200, 2006. https://doi.org/10.1016/j.dental.2005.04.016
  11. Nakamura T, Wakabayashi K, Zaima C, Nishida H, Kinuta S, Yatani H. Tensile bond strength between tooth-colored porcelain and sandblasted zirconia framework. J Prosthodont Res, 53, 116-119, 2009. https://doi.org/10.1016/j.jpor.2009.02.007
  12. Sailer I, Feher A, Filser F, Gauckler LJ, Luthy H, Hammerle CHF. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures. Int J Prosthodont, 20, 383-388, 2007.
  13. Sailer I, Feher A, Filser F, Luthy H, Gauckler LJ, Scharer P, Hammerle CHF. Prospective clinical study of zirconia posterior fixed partial dentures: 3-year follow-up. Quintessence Int, 37, 41-49, 2006.
  14. Sato H, Yamada K, Pezzotti G, Nawa M, Ban S. Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment. Dent Mater J, 27, 408-414, 2008. https://doi.org/10.4012/dmj.27.408
  15. Tada K, Sato T, Yoshinari M. Influence of surface treatment on bond strength of veneering ceramics fused to zirconia. Dent Mater J, 31 (2), 287-96, 2012. https://doi.org/10.4012/dmj.2011-163

Cited by

  1. 소결 전 지르코니아 표면처리와 라이너 사용에 따른 지르코니아와 열가압성형도재의 전단결합강도 vol.37, pp.3, 2015, https://doi.org/10.14347/kadt.2015.37.3.121
  2. 치과용 지르코니아 표면처리방법에 따른 지르코니아와 전장용 도재의 결합강도 관찰 vol.41, pp.4, 2013, https://doi.org/10.14347/kadt.2019.41.4.279