비포름알데하이드계 수지 가공제 처리한 레이온직물의 물리화학적 특성 변화와 최적 처리 조건에 관한 연구

Physicochemical Properties of Non-Formaldehyde Resin Finished Rayon Fabric and Their Optimal Treatment Condition

  • Kim, Han-Gi (Department of Textile System Engineering, Kyungpook National University) ;
  • Yoon, Nam-Sik (Department of Textile System Engineering, Kyungpook National University) ;
  • Huh, Man-Woo (Kyungil University) ;
  • Jeon, Sung-Ki (Korea Dyeing & Finishing Technology Institute)
  • 투고 : 2012.08.27
  • 심사 : 2012.09.21
  • 발행 : 2012.09.27

초록

Rayon fabrics were treated with some commercial non-formaldehyde and low-formaldehyde resins, and then their effect on the physicochemical properties of fabrics, including formaldehyde release, tear strength, shrinkage, and wrinkle recovery, were investigated respectively. Rayons treated with non-formaldehyde resin, little formaldehyde release was observed. Considering other factors, the optimal concentration of non-formaldehyde resin was shown to be 11-13%, and curing temperature was $170{\sim}175^{\circ}C$. In case of low-formaldehyde type, 9-11% resin concentration and curing temperature of $170{\sim}180^{\circ}C$ were recommended for optimal finishing condition. The choice and combination of resins and catalysts were also important factors, and preliminary considerations before resin-finishing of rayon are also important to get much better results.

키워드

참고문헌

  1. Y. H. Kim and K. H. Song, Shrink Proof Finish of Viscose Rayon Fabrics with Cellulose Reactant Resins, Journal of Korean Fiber Society, 33(1), 51(1996).
  2. Y. A. Kwon, Durable Press Performance and Water Repellency of Cotton/Polyester Fabrics Finished by DMDHEU/Fluorochemicals, Textile Coloration and Finishing(J. Korean Soc. Dyers & Finishers), 10(5), 24(1998).
  3. W. D. Schindler and P. J. Hauser, "Chemical Finishing of Textiles", Woodhead Publishing in Textiles, Cambridge, pp.51-72, 2004.
  4. M. Hashem, N. A. Ibrahim, A. El-Shafei, R. Refaie and P. Hauser, An Eco-friendly Novel Approach for Attaining Wrinkle-free/Soft-hand Cotton Fabric, Carbohydrate Polymers, 78(4), 690(2009). https://doi.org/10.1016/j.carbpol.2009.06.004
  5. BASF, "Textile Finishing Published by Manual, D-6700", Federal Republic of Germany, Ludwigshafen, B.360e, No.11, pp.17-46, 1973.
  6. M. Lewin and S. B. Sello, "Handbook of Fiber Science and Technology: Vol II, PART A", Marcel Dekker, USA, pp.34-194, 1983.
  7. H. A. Petersen, "Crosslinking with Formaldehyde-Containing Reactants, in Chemical Processing of Fibers and Fabrics: Functional Finishes, Part A", M. Lewin, and S. B. Sello, Eds., Marcel Dekker, New York, pp.47-327, 1983.
  8. I. Holme, Development in Cross-linking Agents and Catalysts, International Dyer, 191(1), 8(2006).
  9. C. Q. Yang and W. Wei, Evaluating Glutaraldehyde as a Non Formaldehyde Durable Press Finishing Agent for Cotton Fabrics, Textile Research Journal, 70(3), 230(2000). https://doi.org/10.1177/004051750007000309
  10. C. Q. Yang and D. Wang, Evaluating Ester Crosslinking of Cotton Fabric by a Polycarboxylic Acid Using Acid-Base Titration, Textile Research Journal, 70(7), 615(2000). https://doi.org/10.1177/004051750007000709
  11. C. Q. Yang, W. Wei and G. C. Lickfield, Mechanical Strength of Durable Press Finished Cotton Fabric Part III: Change in Cellulose Molecular Weight, Textile Research Journal, 70(10), 910(2000). https://doi.org/10.1177/004051750007001010
  12. Y. L. Lam, C. W. Kan and C. W. Yuen, Wrinkleresistant Finishing with Dimethyloldihydroxyethyleneurea(DMDHEU)-The Effect of Co-catalyst, Textile Research Journal, 81(14), 1419(2010).
  13. Y. H. Park, Scavenger Treatment for Reducing Formaldehyde Content in Resin-Finished Fabrics, Journal of the Korean Society of Textile Engineers and Chemists, 23(3), 39(1986).
  14. J. H. Chung and Y. H. Kim, Low Formaldehyde DP Finish of Polyester/Cotton Blended Fabric, Journal of Korean Fiber Society, 30(8), 600(1993).
  15. Y. L. Lam, C. W. Kan and C. W. M. Yuen, Wrinkle-resistant Finishing of Cotton Fabric with BTCA -The Effect of Co-catalyst, Textile Research Journal, 81(5), 482(2010).
  16. X. Gu and C. Q. Yang, FTIR Spectroscopy Study of the Formation of Cyclic Anhydride Intermediates of Polycarboxylic Acids Catalyzed by Sodium Hypophosphite, Textile Research Journal, 70(1), 64(2000). https://doi.org/10.1177/004051750007000110
  17. S. B. Vukusic, DP Finishing with Polycarboxylic Acids and Phosphono-based Catalyst, AATCC Review, 10(1), 14(2002).
  18. H. S. Cho, B. S. Lee, S. H. Jeong, and E. S. Lee, Effect of Additives for Glyoxal/Aluminium Sulfate in Durable Press Finish of Cotton Fabrics, Textile Science and Engineering, 43(4), 172(2006).
  19. C. C. Chen and C. C. Wang, Crosslinking of Cotton Cellulose with Succinic Acid in the Presence of Titanium Dioxide Nano-catalyst under UV Irradiation, Journal of Sol-Gel Science and Technology, 40(1), 38(2006).
  20. H. G. Kim, N. S. Yoon, M. W. Huh, and I. S. Kim, Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and Their Optimal Treatment Condition, Textile Coloration and Finishing(J. Korean Soc. Dyers & Finishers), 24(2), 121(2012). https://doi.org/10.5764/TCF.2012.24.2.121
  21. C. M. Welch and G. F. Danna, Glyoxal as a Non-Nitrogenous Formaldehyde-Free Durable-Press Reagent for Cotton, Textile Research Journal, 52(2), 149(1982). https://doi.org/10.1177/004051758205200209
  22. C. M. Welch and G. F. Danna, Glyoxal as a Formaldehyde-Free Durable-Press for Mild Curing Applications, Textile Research Journal, 53(3), 181(1983). https://doi.org/10.1177/004051758305300307
  23. C. Q. Yang, L. Qian and G. C. Lickfield, Mechanical Strength of Durable Press Finished Cotton Fabric, Textile Research Journal, 70(2), 148(2000). https://doi.org/10.1177/004051750007000210
  24. C. Q. Yang, L. Qian and G. C. Lickfield, Mechanical Strength of Durable Press Finished Cotton Fabric, Part IV: Abrasion Resistance, Textile Research Journal, 71(6), 543(2001). https://doi.org/10.1177/004051750107100612
  25. I. S. Kang and H. S. Bae, Mechanical Properties of Cotton Fabric Treated with Succinic Acid-Tear Strength, Textile Coloration and Finishing(J. Korean Soc. Dyers & Finishers), 21(3), 1(2009).

피인용 문헌

  1. Improvement of Binding Property of the Alg-Na/PEO Blends vol.26, pp.1, 2014, https://doi.org/10.5764/TCF.2014.26.1.32