Abstract
Various geosynthetics are widely applied to civil structures and waste landfill site for reinforcement and water resistance. The use of geosynthetics inevitably involves the coupled behaviors of different materials which include large displacement and strain-softening behaviors, etc. In this study, the effect of chemical element in the leachate on the interface shear strength under the cyclic loading condition was analyzed. The Multi-purpose Interface Apparatus (M-PIA) has been modified and cyclic direct shear tests have been performed. The submerging period of each specimen is 200 days. Additionally, the Field-Emission Scanning Electronic Microscopy (FIB) analysis has been also performed to induce the reason of the variation of disturbance function and verify the hypothesis on the decay-proof ability of geosynthetics. Consequently, the charateristics of chemical degradation of geosynthetic-soil interface are verified and the variation of the disturbance function is mainly caused by the different type of soil mineral decay, based on the FIB results.
최근 쓰레기 매립장에 널리 사용되고 있는 토목섬유는 흙과의 접촉면에서 대변형 거동 및 변형율 연화 등의 전단거동 특성을 보이는데, 이는 토목섬유-흙 접촉면에서 함수비, 연직응력, 화학적 요소의 영향 등 고유물성에 기인한다. 본 연구에서는 침출수 내의 산성 및 염기성과 같은 성분의 영향이 진동하중 상태에서 토목섬유-흙 접촉면의 전단강도 감소에 미치는 영향을 분석하였다. 이를 위하여 이미 구축된 다기능 접촉면 시험기(M-PIA)를 수정 제작하고 200일간 수침시킨 토목섬유와 흙 시료를 이용하여 진동 직접전단시험을 수행하였고, 그 결과 교란상태개념에 기초하여 화학적 인자들에 의한 토목섬유-흙 접촉면의 화학적 전단강도 감소 특성을 교란도 함수로써 확인하였다. 또한 전계방출주사현미경(FIB)을 이용하여 화학적 인자에 따른 흙입자 및 접촉면 손상의 차이를 확인하였다.