Influence of sandblasting and primer on shear bond strength of resin cement to zirconia

샌드블라스팅과 프라이머가 지르코니아와 레진시멘트의 전단결합강도에 미치는 영향

  • Lee, Jung-Haeng (Department of Prosthodontics, Division of Dentistry, Graduate School, Kyung-Hee University) ;
  • Kim, Hyeong-Seob (Department of Prosthodontics, Division of Dentistry, Graduate School, Kyung-Hee University) ;
  • Pae, Ah-Ran (Department of Prosthodontics, Division of Dentistry, Graduate School, Kyung-Hee University) ;
  • Woo, Yi-Hyung (Department of Prosthodontics, Division of Dentistry, Graduate School, Kyung-Hee University)
  • 이정행 (경희대학교 치과대학 치과보철학교실) ;
  • 김형섭 (경희대학교 치과대학 치과보철학교실) ;
  • 배아란 (경희대학교 치과대학 치과보철학교실) ;
  • 우이형 (경희대학교 치과대학 치과보철학교실)
  • Received : 2010.12.09
  • Accepted : 2011.01.08
  • Published : 2011.01.31

Abstract

Purpose: The aim of this study was to evaluate the effect of mechanical, chemical surface treatments on the zirconia-to-resin cement shear bond strength (SBS). Materials and methods: Eighty zirconia discs (Lava, 3M ESPE) and eighty zirconia/alumina composite (Zirace, Acucera) were embedded in an epoxy resin base. Zirconia discs were randomly divided in to four treatment groups(10 for each manufacturer): $50\;{\mu}m$ $Al_2O_3$ sandblasting (S50), $110\;{\mu}m$ $Al_2O_3$ sandblasting (S110), $50\;{\mu}m$ $Al_2O_3$ and primer (Z-Prime Plus, Bisco Inc) (S50z) and $110\;{\mu}m$ $Al_2O_3$ and primer (Z-Prime Plus) (S110z). Two resin-based luting cements (Calibra, Panavia F) were used to build 2 mm diameter cylinders onto the zirconia. After 24 h of storage in water, SBS testing was evaluate using a universal testing machine. Bond strength data were analyzed with one-way ANOVA, two-way ANOVA test and post hoc comparison was done using Tukey test (${\alpha}$ = .05). Results: Groups using primer showed the high shear bond strength. The groups that did not use primer presented lower shear bond strengths. Conclusion: The use of primer (Z-Prime Plus, Bisco) had significantly higher shear bond strengths.

연구 목적: 최근 지르코니아가 전부도재관의 코어로 많이 사용되고 있다. 지르코니아와 레진 시멘트의 결합 강도를 높이기 위한 기계적, 화학적인 표면 처리 방법들이 연구되고 있다. 이 연구에서 여러 표면 처리 방법에 따른 지르코니아와 레진 시멘트의 전단결합강도를 알아보고자 한다. 연구 재료 및 방법: 80개의 지르코니아 (Lava, 3M ESPE, St. Paul, MN, USA) 시편과 80개의 지르코니아/알루미나 복합체 (Zirace, Acucera Co Inc, Korea) 시편을 디스크형태로 제작하여 에폭시레진에 매립하였다. 이들을 각각 4개의 군으로 나누어 $50\;{\mu}m$ $Al_2O_3$ sandblasting, $110\;{\mu}m$ $Al_2O_3$ sandblasting, $50\;{\mu}m$ $Al_2O_3$ sandblasting과 프라이머 (Z-PRIME Plus, Bisco Inc, Schaumburg, IL, USA) 사용, $110\;{\mu}m$ $Al_2O_3$ sandblasting과 프라이머 (Z-PRIME Plus) 사용 군으로 나누었다. 표면 처리한 지르코니아 표면에 2가지 레진 시멘 (Calibra, Panavia F)으로 접착하였다. 그 후 증류수 ($37^{\circ}C$)에 24시간 보관 후 전단 결합 강도 실험을 시행하였고, SEM을 사용하여 표면 처리한 표면과 전단강도 실험 후 파절양상을 관찰하였다. 결과: ANOVA분석에 따르면, 두 가지 종류의 시편 모두에서, 프라이머 (Z-PRIME Plus)를 사용하여 표면 처리한 군들이 전단 결합 강도가 높았다 (P < .05). 결론: 기계적 결합 강도와 함께 새로운 프라이머를 사용하는 것이 지르코니아와 레진 시멘트의 접착 강도를 증가시킨다.

Keywords

References

  1. Blatz MB, Sadan A, Kern M. Resin-ceramic bonding: a review of the literature. J Prosthet Dent 2003;89:268-74. https://doi.org/10.1067/mpr.2003.50
  2. Blatz MB, Chiche G, Holst S, Sadan A. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia. Quintessence Int 2007;38:745-53.
  3. Luthardt RG, Holzhu¨ter M, Sandkuhl O, Herold V, Schnapp JD, Kuhlisch E, Walter M. Reliability and properties of ground YTZP- zirconia ceramics. J Dent Res 2002;81:487-91. https://doi.org/10.1177/154405910208100711
  4. Luthardt R, Weber A, Rudolph H, Scho¨ne C, Quaas S, Walter M. Design and production of dental prosthetic restorations: basic research on dental CAD/CAM technology. Int J Comput Dent 2002;5:165-76.
  5. Kakehashi Y, Lu¨thy H, Naef R, Wohlwend A, Scha ¨rer P. A new all-ceramic post and core system: clinical, technical, and in vitro results. Int J Periodontics Restorative Dent 1998;18:586-93.
  6. Meyenberg KH, Luthy H, Scharer P. Zirconia posts: a new allceramic concept for nonvital abutment teeth. J Esthet Dent 1995; 7:73-80. https://doi.org/10.1111/j.1708-8240.1995.tb00565.x
  7. Yildirim M, Fischer H, Marx R, Edelhoff D. In vivo fracture resistance of implant-supported all-ceramic restorations. J Prosthet Dent 2003;90:325-31. https://doi.org/10.1016/S0022-3913(03)00514-6
  8. Glauser R, Sailer I, Wohlwend A, Studer S, Schibli M, Scha rer P. Experimental zirconia abutments for implant-supported single-tooth restorations in esthetically demanding regions: 4-year results of a prospective clinical study. Int J Prosthodont 2004;17:285-90.
  9. Derand P, Derand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 2000;13:131-5.
  10. Ozcan M, Vallittu PK. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 2003;19:725-31. https://doi.org/10.1016/S0109-5641(03)00019-8
  11. Zhang Y, Lawn BR, Malament KA, Van Thompson P, Rekow ED. Damage accumulation and fatigue life of particle-abraded ceramics. Int J Prosthodont 2006;19:442-8.
  12. Zhang Y, Lawn BR, Rekow ED, Thompson VP. Effect of sandblasting on the long-term performance of dental ceramics. J Biomed Mater Res B Appl Biomater 2004;71:381-6.
  13. Wolfart M, Lehmann F, Wolfart S, Kern M. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater 2007;23:45-50. https://doi.org/10.1016/j.dental.2005.11.040
  14. Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 1998;14:64-71. https://doi.org/10.1016/S0109-5641(98)00011-6
  15. Blatz MB, Sadan A, Martin J, Lang B. In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconiumoxide ceramic after long-term storage and thermal cycling. J Prosthet Dent 2004;91:356-62. https://doi.org/10.1016/j.prosdent.2004.02.001
  16. Atsu SS, Kilicarslan MA, Kucukesmen HC, Aka PS. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 2006;95:430-6. https://doi.org/10.1016/j.prosdent.2006.03.016
  17. Tanaka R, Fujishima A, Shibata Y, Manabe A, Miyazaki T. Cooperation of phosphate monomer and silica modification on zirconia. J Dent Res 2008;87:666-70. https://doi.org/10.1177/154405910808700705
  18. Tsuo Y, Yoshida K, Atsuta M. Effects of alumina-blasting and adhesive primers on bonding between resin luting agent and zirconia ceramics. Dent Mater J 2006;25:669-74. https://doi.org/10.4012/dmj.25.669
  19. Aida M, Hayakawa T, Mizukawa K. Adhesion of composite to porcelain with various surface conditions. J Prosthet Dent 1995; 73:464-70. https://doi.org/10.1016/S0022-3913(05)80076-9
  20. Luthy H, Loeffel O, Hammerle CH. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 2006;22:195-200. https://doi.org/10.1016/j.dental.2005.04.016
  21. Akgungor G, Sen D, Aydin M. Influence of different surface treatments on the short-term bond strength and durability between a zirconia post and a composite resin core material. J Prosthet Dent 2008;99:388-99. https://doi.org/10.1016/S0022-3913(08)60088-8
  22. Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2000;2:139-47.
  23. Matinlinna JP, Heikkinen T, Ozcan M, Lassila LV, Vallittu PK. Evaluation of resin adhesion to zirconia ceramic using some organosilanes. Dent Mater 2006;22:824-31. https://doi.org/10.1016/j.dental.2005.11.035
  24. Kern M, Thompson VP. Sandblasting and silica coating of a glass-infiltrated alumina ceramic: volume loss, morphology, and changes in the surface composition. J Prosthet Dent 1994;71:453- 61. https://doi.org/10.1016/0022-3913(94)90182-1
  25. Della Bona A, Borba M, Benetti P, Cecchetti D. Effect of surface treatments on the bond strength of a zirconia-reinforced ceramic to composite resin. Braz Oral Res 2007;21:10-5. https://doi.org/10.1590/S1806-83242007000100002
  26. Uo M, Sjo¨gren G, Sundh A, Goto M, Watari F, Bergman M. Effect of surface condition of dental zirconia ceramic (Denzir) on bonding. Dent Mater J 2006;25:626-31. https://doi.org/10.4012/dmj.25.626
  27. Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. Strength and reliability of surface treated Y-TZP dental ceramics. J Biomed Mater Res 2000;53:304-13. https://doi.org/10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S
  28. Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 2005;33:9-18. https://doi.org/10.1016/j.jdent.2004.07.001
  29. Wang H, Aboushelib MN, Feilzer AJ. Strength influencing variables on CAD/CAM zirconia frameworks. Dent Mater 2008; 24:633-8. https://doi.org/10.1016/j.dental.2007.06.030
  30. Karakoca S, Yilmaz H. Influence of surface treatments on surface roughness, phase transformation, and biaxial flexural strength of Y-TZP ceramics. J Biomed Mater Res B Appl Biomater 2009;91:930-7.
  31. Kern M, Thompson VP. Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability. J Prosthet Dent 1995;73:240-9. https://doi.org/10.1016/S0022-3913(05)80200-8
  32. Tanaka T, Nagata K, Takeyama M, Atsuta M, Nakabayashi N, Masuhara E. 4-META opaque resin-a new resin strongly adhesive to nickel-chromium alloy. J Dent Res 1981;60:1697-706. https://doi.org/10.1177/00220345810600091101
  33. Lindgren J, Smeds J, Sjo¨gren G. Effect of surface treatments and aging in water on bond strength to zirconia. Oper Dent 2008; 33:675-81. https://doi.org/10.2341/08-12
  34. Silikas N, Wincott PL, Vaughan D, Watts DC, Eliades G. Surface characterization of precious alloys treated with thione metal primers. Dent Mater 2007;23:665-73. https://doi.org/10.1016/j.dental.2006.06.007
  35. Ozcan M, Nijhuis H, Valandro LF. Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging. Dent Mater J 2008;27:99-104. https://doi.org/10.4012/dmj.27.99
  36. Magne P, Paranhos MP, Burnett LH Jr. New zirconia primer improves bond strength of resin-based cements. Dent Mater 2010;26:345-52. https://doi.org/10.1016/j.dental.2009.12.005
  37. Wang H, Aboushelib MN, Feilzer AJ. Strength influencing variables on CAD/CAM zirconia frameworks. Dent Mater 2008; 24:633-8. https://doi.org/10.1016/j.dental.2007.06.030

Cited by

  1. The effect of resin cements and primer on retentive force of zirconia copings bonded to zirconia abutments with insufficient retention vol.5, pp.2, 2013, https://doi.org/10.4047/jap.2013.5.2.198
  2. Understanding and trends of esthetic treatment in prosthodontics : part 2. Zirconia vol.14, pp.5, 2014, https://doi.org/10.13065/jksdh.2014.14.05.617
  3. 지르코니아의 다양한 표면처리 방법과 레진시멘트 종류에 따른 전단결합강도 비교 vol.59, pp.2, 2021, https://doi.org/10.4047/jkap.2021.59.2.153