olymerization behavior and thermal characteristics of two new composites at five temperatures: refrigeration to preheating

  • Jafarzadeh-Kashi, Tahereh Sadat (Department of Dental Materials, Faculty of Dentistry, Tehran University of Medical Sciences, Research Center for Medical and Technology in Medical Sciences, Tehran University of Medical Sciences) ;
  • Mirzaii, Marzieh (Department of Pharmaceutics, Pharmacy School, Shahid Beheshti University of Medical Sciences) ;
  • Erfan, Mohmmad (Department of Pharmaceutics, Pharmacy School, Shahid Beheshti University of Medical Sciences) ;
  • Fazel, Akbar (Department of Prosthodontics, Faculty of Dentistry, Tehran University of Medical Sciences, Secretary of the Dentistry and Specialties, Deputy of Education, Ministry of Health and Medical Education) ;
  • Eskandarion, Solmaz (Department of Dental Materials, Faculty of Dentistry, Tehran University of Medical Sciences) ;
  • Rakhshan, Vahid (Department of Dental Anatomy and Morphology, Dental Branch, Islamic Azad University)
  • Received : 2011.10.20
  • Accepted : 2011.11.24
  • Published : 2011.12.30

Abstract

PURPOSE. Heat of composite polymerization (HP) indicates setting efficacy and temperature increase of composite in clinical procedures. The purpose of this in vitro experimental study was to evaluate the effects of 5 temperatures on HP of two new composites. MATERIALS AND METHODS. From each material (Core Max II [CM] and King Dental [KD]), 5 groups of 5 specimens each were prepared and their total HPs (J/gr) were measured and recorded, at one of the constant temperatures $0^{\circ}C$, $15^{\circ}C$, $23^{\circ}C$, $37^{\circ}C$ and $60^{\circ}C$ ($2{\times}5{\times}5$ specimens) using a differential scanning calorimetry (DSC) analyzer. The data were analyzed using a two-way ANOVA, a Tukey's test, an independent-samples ttest, and a linear regression analysis (${\alpha}=0.05$). RESULTS. No polymerization reactions occurred at $0^{\circ}C$; then this temperature was excluded from statistical analyses. The mean HP of the remaining 20 KD specimens was $20.5{\pm}14.9$ J/gr, while it was $40.7{\pm}12.9$ J/gr for CM. The independent-samples t-test showed that there were significant differences between the HP of the two materials at the temperatures $15^{\circ}C$ (P=.0001), $23^{\circ}C$ (P=.0163), $37^{\circ}C$ (P=.0039), and $60^{\circ}C$ (P=.0106). Linear regression analysis showed statistically significant correlations between environment temperatures and HP of CM ($R^2=0.777$). CONCLUSION. Using CM is advantageous over conventional composite because of its better polymerization capacity. However due to its high HP, further studies should assess its temperature increase in vivo. Preheating KD is recommended. Refrigerating composites can negatively affect their polymerization potential.

Keywords

References

  1. Shillingburg HT, Hobo S, Whitsett LD, Jacobi R, Brackett SE. Fundamentals of fixed prosthodontics. Chicago: Quintessence Publishing; 1997.
  2. Kovarik RE, Breeding LC, Caughman WF. Fatigue life of three core materials under simulated chewing conditions. J Prosthet Dent 1992;68:584-90. https://doi.org/10.1016/0022-3913(92)90370-P
  3. Antonucci JM, Toth EE. Extent of polymerization of dental resins by differential scanning calorimetry. J Dent Res 1983;62:121-5. https://doi.org/10.1177/00220345830620020701
  4. Prasanna N, Pallavi Reddy Y, Kavitha S, Lakshmi Narayanan L. Degree of conversion and residual stress of preheated and roomtemperature composites. Indian J Dent Res 2007;18:173-6. https://doi.org/10.4103/0970-9290.35827
  5. Cotti E, Scungio P, Dettori C, Ennas G. Comparison of the Degree of Conversion of Resin Based Endodontic Sealers Using the DSC Technique. Eur J Dent 2011;5:131-8.
  6. Daronch M, Rueggeberg FA, De Goes MF. Monomer conversion of pre-heated composite. J Dent Res 2005;84:663-7. https://doi.org/10.1177/154405910508400716
  7. Awliya WY. The influence of temperature on the efficacy of polymerization of composite resin. J Contemp Dent Pract 2007;8:9-16.
  8. Faria-E-Silva AL, Piva E, Moraes RR. Time-dependent effect of refrigeration on viscosity and conversion kinetics of dental adhesive resins. Eur J Dent 2010;4:150-5.
  9. Daronch M, Rueggeberg FA, Moss L, de Goes MF. Clinically relevant issues related to preheating composites. J Esthet Restor Dent 2006;18:340-50; discussion 351. https://doi.org/10.1111/j.1708-8240.2006.00046.x
  10. Lohbauer U, Zinelis S, Rahiotis C, Petschelt A, Eliades G. The effect of resin composite pre-heating on monomer conversion and polymerization shrinkage. Dent Mater 2009;25:514-9. https://doi.org/10.1016/j.dental.2008.10.006
  11. Choudhary N, Kamat S, Mangala T, Thomas M. Effect of preheating composite resin on gap formation at three different temperatures. J Conserv Dent 2011;14:191-5. https://doi.org/10.4103/0972-0707.82618
  12. Driscoll CF, Woolsey G, Ferguson WM. Comparison of exothermic release during polymerization of four materials used to fabricate interim restorations. J Prosthet Dent 1991;65:504-6. https://doi.org/10.1016/0022-3913(91)90289-9
  13. Hussey DL, Biagioni PA, McCullagh JJ, Lamey PJ. Thermographic assessment of heat generated on the root surface during post space preparation. Int Endod J 1997;30:187-90. https://doi.org/10.1111/j.1365-2591.1997.tb00695.x
  14. Lipski M. Root surface temperature rises during root canal obturation, in vitro, by the continuous wave of condensation technique using System B HeatSource. Oral Surg Oral Med Oral Pathol Oral Radiol Endod 2005;99:505-10. https://doi.org/10.1016/j.tripleo.2004.07.014
  15. Behnia A, McDonald NJ. In vitro infrared thermographic assessment of root surface temperatures generated by the thermafil plus system. J Endod 2001;27:203-5. https://doi.org/10.1097/00004770-200103000-00016
  16. Atai M, Ahmadi M, Babanzadeh S, Watts DC. Synthesis, characterization, shrinkage and curing kinetics of a new low-shrinkage urethane dimethacrylate monomer for dental applications. Dent Mater 2007;23:1030-41. https://doi.org/10.1016/j.dental.2007.03.004
  17. Lee H, Colby C. Heat of polymerization of nine mono-, di-, and trimethacrylate esters tested neat and with low levels of peroxide by dynamic differential scanning calorimetry. Dent Mater 1986;2:175-8. https://doi.org/10.1016/S0109-5641(86)80031-8
  18. MartIn JL. Kinetic analysis of an asymmetrical DSC peak in the curing of an unsaturated polyester resin catalysed with MEKP and cobalt octoate, Polymer 1999;40:3451-62. https://doi.org/10.1016/S0032-3861(98)00556-4
  19. Tanimoto Y, Hayakawa T, Nemoto K. Analysis of photopolymerization behavior of UDMA/TEGDMA resin mixture and its composite by differential scanning calorimetry. J Biomed Mater Res B Appl Biomater 2005;72:310-5.
  20. Atai M, Motevasselian F. Temperature rise and degree of photopolymerization conversion of nanocomposites and conventional dental composites. Clin Oral Investig 2009;13:309-16. https://doi.org/10.1007/s00784-008-0236-2
  21. Chung KH, Greener EH. Correlation between degree of conversion, filler concentration and mechanical properties of posterior composite resins. J Oral Rehabil 1990;17:487-94. https://doi.org/10.1111/j.1365-2842.1990.tb01419.x
  22. Guiraldo RD, Consani S, De Souza AS, Consani RL, Sinhoreti MA, Correr-Sobrinho L. Influence of light energy density on heat generation during photoactivation of dental composites with different dentin and composite thickness. J Appl Oral Sci 2009;17:289-93. https://doi.org/10.1590/S1678-77572009000400005
  23. Bayne SC, Thompson JY. Biomaterials. In: Roberson TM, Heymann HO, Ritter AV, eds. Sturdevant's art and science of operative dentistry. St. Louis: The CV Mosby Co.; 2006. p. 135-242.
  24. Pojman JA, Ilyashenko VM, Khan AM. Free-radical frontal polymerization: self-propagating thermal reaction waves. J Chem Soc Faraday Trans 1996;92:2825-37. https://doi.org/10.1039/ft9969202825
  25. Daronch M, Rueggeberg FA, Hall G, De Goes MF. Effect of composite temperature on in vitro intrapulpal temperature rise. Dent Mater 2007;23:1283-8. https://doi.org/10.1016/j.dental.2006.11.024
  26. Tantbirojn D, Chongvisal S, Augustson DG, Versluis A. Hardness and postgel shrinkage of preheated composites. Quintessence Int 2011;42:e51-9.

Cited by

  1. Microstructure and Mechanical Properties of Composite Resins Subjected to Accelerated Artificial Aging vol.24, pp.6, 2013, https://doi.org/10.1590/0103-6440201302263
  2. The effects of dentin bonding agent formulas on their polymerization quality, and together with tooth tissues on their microleakage and shear bond strength: an explorative 3-step experiment vol.6, pp.5, 2014, https://doi.org/10.4047/jap.2014.6.5.333
  3. Mechanical properties of composites as functions of the syringe storage temperature and energy dose vol.23, pp.2, 2015, https://doi.org/10.1590/1678-775720130643
  4. Effects of at-home and in-office bleaching and three composite types (hybrid, microhybrid, and nanofilled) on repair shear bond strength of aged composites: A preliminary study vol.18, pp.1, 2011, https://doi.org/10.4103/1735-3327.324020