Abstract
The current design practice of an electric transmission tower is based on the allowable stress design. Design strengths of the electric transmission tower's compression member are determined by buckling the strength of the member itself without considering joint strength. There is a possibility of a joint failure prior to the buckling of a member. Therefore, in this study, joint strength is calculated for various member forces, and the shape of joint and database of strength were established. These data was compared with the member strength obtained from previous research studies based on an equivalent nonlinear analysis technique. Finally, practical evaluation and design method to distinguish failure mode in an electric transmission tower member is proposed.
현행 송전강관철탑의 경우 허용응력 설계개념을 도입한 철탑설계기준을 적용하여 설계, 제작되고 있다. 이 철탑설계기준의 압축재의 설계 강도 결정은 압축재의 허용좌굴응력에 의하여 결정되고 있으나 이는 접합부의 내력을 고려치 않은 값이다. 부재가 압축좌굴내력에 도달하기 전에 접합부의 변형으로 인하여 국부변형에 의한 접합부 파괴가 발생할 수 있다. 따라서 본 연구에서는 접합부의 보강형태별로 접합부내력을 산출하고 이를 데이터베이스화한 후 지난 연구에서 도출한 등가비선형해석기법의 부재내력과의 상호 비교를 통하여 부재파괴와 접합부파괴의 선행 여부를 판별할 수 있는 실용적인 평가 및 설계 기법을 제시하였다.