Sialon was produced by hot-pressing the mixtures of $Si_3N_4$, AlN and $Y_2O_3$ powders. All fracture tests were performed on a three-point loading system with a 30 mm bending span. Fracture toughness and Vickers hardness of smooth specimen were average 7.05 $MPa{\cdot}m^{0.5}$ and Hv = 1580, respectively. Density of three kinds of specimens, smooth specimen, smooth and healed specimen, smooth with $SiO_2$ colloidal coating and healed specimen, had beyond 99 % of theoretical density. Bending strength of smooth healed specimens had high strength more than 1 GPa. Crack healed specimens recovered as strength as smooth specimen. That is, cracked specimen with $SiO_2$ colloidal coating on cracked part recovered strength by heat treatment, completely. Crack healing of $Si_3N_4$ composite ceramics had contributed glassy $SiO_2$ to strength recovery. Limiting high temperature for bending strength of heat treated smooth specimen for bending strength was about 1273 K.

Keywords

References

  1. Sakano, H. and Asano, K., 1987, 'Ceramics for Automobile,' Sankaido, p. 180
  2. Kijima, K. and Shirasaki, S., 1976, 'Nitrogen Self-Diffusion in Silicon Nitride,' Journal of Chemical Physics, Vol. 65, pp. 2668∼2671 https://doi.org/10.1063/1.433464
  3. Lange, F.F., 1980, 'Silicon Nitride Systems: Fabrication Microstructure, and Properties,' Int. Metals Rev. Vol. 247, No. 1, pp. 1-20
  4. Lange, F.F., 1983, 'Fabrication and Properties of Dense Polyphase Silicon Nitride,' Bull. Am. Ceram. Soc., Vol. 62, No. 12, pp. 1369-74
  5. Nam, K.W., Moon, S.J., Park, S.W., Ahn, S.H. and Kim, J.S., 2007, 'Characteristics of Sialon by Additive Al2O3 and Y2O3,' Proceeding of The KSPSE 2007 Fall Annual Meeting, pp. 262-267
  6. Jack, K.H., 1976, 'Sialons and Related Nitrogen Ceramics,' J. Mater. Sci., Vol. 11, pp. 1135-58 https://doi.org/10.1007/BF02396649
  7. Jack, K.H. and Wilson, W.I., 1972, 'Ceramics Based on Silicon Nitride,' Nature Physical Science, Vol. 238, No. 28, pp. 128-129
  8. Nam, K.W., Kim, M.K., Park, S.W., Ahn, S.H. and Kim, J.S., 2007, 'Crack Healing Behavior and Bending Strength of $Si_3N_4$/SiC Composite Ceramics by SiO2 Colloidal,' Mater. Sci. and Engng. A, Vol. 471, pp. 102-105. https://doi.org/10.1016/j.msea.2007.03.005
  9. Nam, K.W., Park, S.W., Ahn, S.H., 2008, 'Crack-healing Behavior and Strength Properties of SiC Ceramics According to Additives $SiO_2$,' Proceeding of Korea Ocean Science Technique Council 2007 Joint Meeting, pp. 2430
  10. Wada, S. and Ukyo, Y., 1989, 'Euro-Ceramics,' Vol. 1, pp. 566-571
  11. Lawn, B.R. and Fuller, E.R., 1975, 'Equilibrium Penny-Like Cracks in Indentation on Fracture,' J. Mater. Sci., Vol. 10, pp. 2016-24 https://doi.org/10.1007/BF00557479
  12. Ye. F., Hohhman. J.M., Holzer. S. and Iwasa. M., 2004, 'Microsstructural Development of Y-$\alpha$/($\beta$)-Sialon after Post Heat-Treatment and its Effect on Mechanical Properties,' Ceramics International, Vol. 30, pp. 229-238 https://doi.org/10.1016/S0272-8842(03)00094-4
  13. Kim, M.K., Park, S.W., Son, C.S., Ahn, S.H. and Nam, K.W., 2006, 'Crack Healing and Bending Strength of $Si_3N_4$/SiC Composite Ceramics by Additive Powder $TiO_2$,' Proceeding of The KSME 2006 Fall Annual Meeting, pp. 149-152
  14. Lee, S.K., Ishida, W., Lee, S.Y., Nam, K.W. and Ando, K., 2005, 'Crack-Healing Behavior and Resultant Strength Properties of Silicon Carbide Ceramic,' J. Eur. Ceram Soc., Vol. 25, No. 5, pp. 569-576 https://doi.org/10.1016/j.jeurceramsoc.2004.01.021
  15. Ando, K., Houjyou, K., Chu, M. C., Takeshita, S., Takahashi, K., Sakamoto, S., 2002, 'Crack-Healing Behavior of $Si_3N_4$/SiC Ceramics under Stress and Fatigue Strength at the Temperature of Healing ($1000^{\circ}C$),' J. Eur. Ceram. Soc. Vol. 22, pp. 1339-1346 https://doi.org/10.1016/S0955-2219(01)00435-6