Evaluation of Life Time for Anti-Corrosive Methods for Marine Steel Sheet by Cyclic Corrosion Test

실내 가속부식시험을 통한 해양 강관합성 말뚝의 방식 기법 수명 평가

  • Park, J.W. (Reaserch Institute of Industrial Science & Technology, Ulsan Laboratory) ;
  • Lee, J.G. (Reaserch Institute of Industrial Science & Technology, Steel Structural Laboratory) ;
  • Lee, K.W. (Reaserch Institute of Industrial Science & Technology, Ulsan Laboratory) ;
  • Kim, J.H. (Reaserch Institute of Industrial Science & Technology, Ulsan Laboratory) ;
  • Jung, M.K. (Korea Institute of Construction Technology, Earth Structure & Foundation Engineering Research Division) ;
  • Lee, J.H. (Korea Institute of Construction Technology, Earth Structure & Foundation Engineering Research Division)
  • 박종원 (포항산업과학연구원 재료공정연구소 울산산업기술연구본부) ;
  • 이종구 (포항산업과학연구원 강구조연구소 토목연구본부) ;
  • 이경황 (포항산업과학연구원 재료공정연구소 울산산업기술연구본부) ;
  • 김진홍 (포항산업과학연구원 재료공정연구소 울산산업기술연구본부) ;
  • 정문경 (한국건설기술연구원 지반연구실) ;
  • 이주형 (한국건설기술연구원 지반연구실)
  • Received : 2009.12.07
  • Accepted : 2009.12.29
  • Published : 2009.12.01

Abstract

When a steel sheet pipe applied to marine environment, an anti-corrosive coating should be treated to obtain long-term life-time for steels, especially, splash zone. Although anti-corrosive property of coatings is required to be tested in real marine environment, it is difficult because of long test time such as 20 years or more time. Therefore, we used cyclic corrosion tester in a laboratory, which has similar conditions with salt-dry-wet process such as real marine environment. Anti-corrosive properties of the coatings and two steels were tested their anti-corrosive properties under cyclic corrosion test conditions(KS D ISO 14993) and the results were compared with estimate life-time in real marine environment. According to cyclic corrosion test, accelerated corrosive factor of each anti-corrosive coating was investigated accelerated corrosive factor from impedance with EIS method. Accelerated corrosive factor of type SS400 carbon steel and A690 was also investigated their accelerated corrosive factor from the regression curves of weigh loss results. One of the anti-corrosive coatings showed about 50 years life-time compared with standard sample life-time. Carbon steel SS400 showed from 0.1 mm/yr to 0.06 mm/yr as its corrosion rate.

Keywords

References

  1. L. G. S. Gray and B. R. Appleman, J. Protective Coating sand Linings, 20, 70 (2003)
  2. B. Stratman, Encyclopedia of electrochemistry, Wiley-VCH Weinheim, 11, 502 (2001)
  3. C. H. Hare, SSPC, 231, 240-241, 249, 254 (2001)
  4. L. G. S. Gray and B. R. Appleman, ICC Proceedings209 (2002)
  5. C. G. Munger, NACE, 2nd ed., p. 381, Houston, Texas,1986
  6. B. R. Appleman, J. Coatings Technology, 62, 57 (1990)
  7. KS D ISO 14993, Korean Standards Association (2003)
  8. G. Bierwagen et. al., Prog. Org. Coat., 46, 148 (2003) https://doi.org/10.1016/S0300-9440(02)00222-9
  9. 藤原 博,田原 芳雄, 土木学会論文集, 563, 39 (1997)
  10. J. Andrews, J. Coatings Technology, 66, 837 (1994)
  11. T. Tomita and N. Kashino, J. Struct. Constr. Eng., 551,39 (1998)
  12. K. Paik, Corrosion and Protection, 4, 46 (2005)