Abstract
The implant prototypes with various porosities were fabricated by Spark Plasma Sintering of atomized spherical titanium balls. The interface was observed by optical microscope. Sintering temperature and holding time were selected at the point of big change of Z-axis ratio during sintering. These experiments show that Spark Plasma Sintering of spherical titanium balls can be efficiently used to produce implants surfaced with titanium balls with various porosities in a short time less than 120 seconds by manipulating the current condition such as z-axis, temperature and balls size.