Improvement of Thermal Stability of Electrospun PAN Fibers by Various Additives

  • Lee, Young-Seak (Department of Fine Chemical Engineering and Chemistry, Chungnam National University) ;
  • Kim, Min-Il (Department of Fine Chemical Engineering and Chemistry, Chungnam National University) ;
  • Im, Ji-Sun (Department of Fine Chemical Engineering and Chemistry, Chungnam National University) ;
  • In, Se-Jin (Department of Fire and Disaster Protection Engineering, Woosong University)
  • Received : 2008.08.12
  • Accepted : 2008.09.16
  • Published : 2008.09.30

Abstract

In order to improve the thermal stability of PAN-based electrospun fibers, AP-PER-MEL and $TiO_2$ were added in to the fibers as additives. The polymer composite with uniformly mixed additional agents was obtained. In case of non-treated sample, the fibers were burn off completely with high rate within $620^{\circ}C$. But in case of treated samples (EF-M and EF-MT), it is sure that the thermal stability was improved by studying TGA data and ISO flammability test about 20 and 30%, respectively. A synergy effect of adding two kinds of agents (AP-PER-MEL and $TiO_2$) into PAN-based electrospun fibers was confirmed. Through SEM images, it is confirmed that the fiber shape can be kept even after addition of agents (AP-PER-MEL and $TiO_2$). Finally the thermal stability of fibers was largely developed with keeping the nature of PAN-based fibers effectively.

Keywords

References

  1. Li, G.; Liang, G.; He, T.; Yang, Q.; Song, X. Polym. Degrad. Stabil. 2007, 92, 569. https://doi.org/10.1016/j.polymdegradstab.2007.01.018
  2. Vandersall, H. L. J. Fire Flamm. 1971, 2, 97.
  3. Rhys, J. A. Fire Mater. 1980, 4, 154. https://doi.org/10.1002/fam.810040308
  4. Zhang, G. C.; Gu, J. W. J. Mater. Eng. 2006, 1, 47.
  5. Duquesnea, S.; Magnetb, S.; Jamaa, C.; Delobelc, R. Surf. Coat. Tech. 2004, 302, 180.
  6. Camino, G.; Costa, L.; Trossarelli, L. Polym. Degrad. Stabil. 1984, 7, 221. https://doi.org/10.1016/0141-3910(84)90098-3
  7. Bertelli, G.; Costa, L.; Fenza, S.; Marchetti, E.; Camino, G.; Locatelli, R. Polym. Degrad. Stabil. 1988, 20, 295. https://doi.org/10.1016/0141-3910(88)90074-2
  8. Xiao, X. C.; Jiang, W. H.; Song, L. X.; Tian J. F.; Hu, X. F. Diam. Relat. Mater. 2000, 9, 1782. https://doi.org/10.1016/S0925-9635(00)00322-8
  9. Im, J. S.; Kwon, O.; Kim, Y. H.; Park, S. J.; Lee, Y. S. Micropor. Mesopor. Mat. 2008, 115, 514. https://doi.org/10.1016/j.micromeso.2008.02.027
  10. Wang, D. Y.; Liu, Y.; Wang, Y. Z.; Artiles, C. P.; Hull, T. R.; Price, D. Polym. Degrad. Stabil. 2007, 92, 1592. https://doi.org/10.1016/j.polymdegradstab.2007.04.015

Cited by

  1. Nanocomposites based on transition metal oxides in polyvinyl alcohol for EMI shielding application vol.71, pp.2, 2014, https://doi.org/10.1007/s00289-013-1073-2