Abstract
Nylon textured yarn is usually manufactured by disk type false twist texturing. Dyeing properties of nylon textured yam have not been studied yet. In this study, dyeing properties of nylon textured yam according to draw ratio out of process parameters were investigated. The fact that microstructure of nylon textured yarn in amorphous region particularly is transformed by draw ratio was confirmed indirectly by measurement of dyeing rate because dyeing rate was affected by the structure of amorphous region. Dyeing rate at draw ratio 1.29 was the lowest because the higher draw ratio increase amorphous orientation and disturb dye diffusion into amorphous region. The microstructure according draw ratio was indirectly confirmed by 5% strength, tenacity, elongation. But difference in K/S value and fastness was insignificant.