Abstract
The results of warmth retaining, heat transfer and compressive elastic recovery of the five kinds of bedspread fabrics, which were produced from packing weft of 2700 denier and 3600 denier batt yarn treated with raw material of Polyester $150^D$/48 DTY, are as follows: 1) 3600 denier packing weft showed lover count in compressive elastic recovery than 2700d packing weft, so it took longer time to recover. 2) When packing weft of the same count is used, a sample of packing weft with higher density showed lower recovery. 3) It took 2700d packing weft 30min to get approximately 98% recovery in temperature $30^{\circ}C$. But, 3600d packing weft stayed under 98% recovery in the same temperature. Considering only the result of compressive elastic recovery, we should use 2700d packing weft. 4) The higher the density of packing weft is, the higher warmth retaining becomes. Although sharp increase appeared until 5min, equilibrium was kept without any increase after that time. 5) When 2700d packing weft was used, the maximum warmth retaining was approximately 60% and 64% in the conditions of density 12(thread/in) and 22(thread/in) respectively.