Corrosion Resistance of Non-Chrome Magni 565 Coating and Characteristics of Its Coating Film

Non-Chrome Magni 565 코팅 피막의 특성과 내식성

  • Received : 2006.07.03
  • Accepted : 2006.07.22
  • Published : 2006.07.30

Abstract

In addition to the basic properties of the base and top coating agents, corrosion resistance of non-chrome magni 565 coating and characteristics of coating film when coated to steel substrate were studied. The system had a good wettability at room temperature. Moreover, both the contact angle and surface tension were affected little by the viscosity of coating agent and surface roughness of the steel substrate. And the samples coated with optimal conditions showed a great corrosion resistance in salt spray test with 1500 hours or longer of initial appearance time of rust. The coating film was composed of overlapping layer of zinc and aluminium flakes, and the thickness of base coat increased with an increase of base coat viscosity. Based on the C-F peaks of 1,1-Difluoroethaen homo-polymer, it was thought that the base coat was an inorganic polymer bond layer. Meanwhile, the top coat showed C-F peaks of polytetrafluoroethylene with C-H peaks of phenol in FT-IR analysis. From the lower weight loss of base coat in TG analysis, it was thought that cross linking density of base coat was larger than that of top coat. It was thought that the small exothermic reactions observed in DSC curves were due to the thermosetting resins contained in the coating agents. Compared to the non-coated specimen, the coated sample showed more higher polarization resistance and corrosion potential with lower corrosion current density.

Keywords

References

  1. Kunt Westphal: Ein optimiertes Beschichtungssystem fur Verbindungselemente, ATZ 107, Heft 5, (2005) 2
  2. 산업자원부 : 자동차 부품의 6가 크롬 대체 표면처리 기술개발 및 적용에 대한 연구 (2005) 5
  3. K. Westphal : Verffentlicht in mo metalloberflache 56, Nr. 5 (2002) 20-23
  4. Knut Westphal, Hermann Kohler: Korrossionsschutz am Automobil, September, 29/30 (2003)
  5. 한국 다크로 공업회 : 다크로(Dacro)처리 핸드 북, 아연말 화성피막처리, 1월 (1996)
  6. Anochrome Ltd.: Design guide, Surface finishing technology, May (2001) 1-19
  7. Metal coatings international, Inc. ; Geomet coating, A completely chromium-free coating, chardon, Ohio USA
  8. Magni Industries, Inc.,: 2771 Hammond, Detroit Michigan, 48209, Material safety data sheet of B06J and B18
  9. The Magni Group, Inc.: Magni 500 series, High-performance Fastener/Hose clamp Coatings, Magni 565
  10. Michel Cartier; Handbook of surface treatments and coatings, Professional engineering publishing (2003) 83-90
  11. 한국 공업 표준 협회 : KS 핸드북, 86-87, 철강 (1986) 192
  12. 李鶴烈 : 金屬腐蝕工學, 淵鏡文化社, (1995) 44
  13. Sang Hyun Kim, Dong Ho Shin etal. : J. Kor. Inst. Met. & Mater., 43 (2005) 538-543
  14. M.G. Kim, B.H Jung et al. : J. of Korean Society for Heat Treatment, 15 (2002) 215
  15. S.J. Park, J.S. Kim and C.W. Nah : Elastomer, 35 (2000) 98-105
  16. EM 1110-2-3400 : Coating type and characteristics, Chapter 4, 30 Apr., (1995) 1-24
  17. X. G. Zhang : Corrosion and electrochemistry of zinc, zinc-rich coatings, Plenum press (1996) 337-349
  18. ASM international: ASM handbook, Corrosion, 13A (2003) 855