초록
In this paper, we describe the luminescent properties of the phosphors synthesized via sol-gel technique. When the phosphor prepared by sol-gel technique, reaction factors, such as pH condition, $R_w$ and drying temperature affected the luminescent intensity, particle size and morphology of final product. Therefore, we attempt to control these reaction factors in order to improve the luminescent efficiency of phosphors. As a result of our study, when the acid catalyst (HCl) was used, emission intensity was higher than the case of base catalyst $(NH_4OH)$. The product prepared at $R_w=60$ indicated the maximum intensity. As the increase of the $R_w$ value, the particle was agglomerated and emission intensity was decreased. Finally, optimum drying temperature of gel was found to be$ 180^{\circ}C$.