Abstract
A laser welding has been made between sintered tip of Fe-Co-W and low carbon steel shank for the diamond saw blade. The welding characteristics and formation of defect has been investigated carefully for the weld fusion zone in different welding condition. Full penetration has been observed for the whole range of heat input investigated in the present work. Bead width and under-fill have been increased with the increase of heat input. With increasing of heat input small cavities were decreased while large cavities were increased. The ratio of total cavity area to the entire weld bead area was not changed significantly with change of heat input. Most of cavities were found near the tip, and supposed to be formed from the pore in the tip.