Abstract
Tension variations with heat treatment in shadow mask for flat braun tubes are investigated in this study. In CRT, landing shift of the electron beam due to thermal deformation of the tension mask made the color purity of screen worse. In order to get the final results of thermal deformation, the tensile force within the mask and the welding processes between the rail and the extended mask have to be analysed sequentially. In this study, the effect of heat treatment is studied in terms of tension variations of shadow mask during its manufacturing process.