Abstract
Recently, miniaturization and mass production are the main trends in manufacturing fields. Therefore, ultraprecision machining and MEMS technology have been taken more 7md more important position in machining of microparts. Micro endmilling is one of the prominent technology that has wide spectrum of application field ranging from duo parts to micro products, such as PDP md IT components, in precision products manufacturing. However, decreasing of burr is significant problem in making smooth and precise parts in micro endmilling. This paper shows removal characteristics of burr generated by micro endmilling process. This results satisfies micro endmilling for micro barrier ribs of heights is $50{\mu}m$, $100{\mu}m$, $200{\mu}m$, $300{\mu}m$, and observation from of burr. Additionally, it is necessary to understand the formation mechanism of burr of micro barrier ribs to iud proper decreasing method.