The monomer N,N'-bis(2-pyrrol-1-yl-propyl)-4,4'-bipyridine(bpb) was electrochemically polymerized on the glassy carbon electrode surface, which was modified with 1:1 ratio of erichrome black T(EBT) and glutathione(GSSG) to give a type of GC/poly-bpb, EBT, GSSG electrode for depositing Zn(II). The diffusion coefficients of the incorporated ions were 2.43${\times}10^{-15}$ and 9.14${\times}10^{-15} cm^2s^{-1}$ before taking Zn(II) ions and after them respectively. The modified electrodes are stable at the electrode process. The polymerized poly-bpb of 2.83${\times}10^4gmol^{-1}$ can deposit 2.15${\times}10^4gmol^{-1}$ of Zn(II). The number of pumping ions involving in the redox procedure at 0.77 V was 81.7% of the captured 180 ions into the polymer matrix, which was 3 times larger than that of the electrode modified with EBT alone.
단량체인 N,N'-bis(2-pyrrol-1-yl-propyl)-4,4'-bipyridine(bpb)을 유리탄소전극 상에 전기화학적으로 중합한 고분자 피막전극을 erichrome black T(EBT) 와 glutathione(GSSG)의 1:1 용액으로 수식하여 GC/poly-bpb, EBT, GSSG형의 전극을 제작하고 이로써 Zn(II)을 포집한 전극을 제작하였다. 수식된 피막 내에서 이온의 확산계수는 아연이온이 포집되기 전후에 각각 2.43${\times}10^{-15}$과 9.14${\times}10^{-15}cm^2s^{-1}$으로 피막내의 전기화학적 활성자리에서 이탈이 거의 일어나지 않는 안정한 전극이다. 중합된 bpb의 양이 2.83${\times}10^4gmol^{-1}$에 대하여 1.17${\times}10^4gmol^{-1}$의 아연이온이 포집되었다. 이들 중에 산화-환원 과정에서 회합/해리에 관여하는 이온은 포집된 180개의 이온들 중에서 81.7%였다. 이는 EBT 만으로 수식된 전극에서 보다 3배정도 큰 값이다.