온도에 따른 탄탈 분말 제조와 특성

Production of Tantalum Powder and Characteristics by Temperature

  • 윤재식 (회유금속 소재 연구소) ;
  • 박형호 (회유금속 소재 연구소) ;
  • 배인성 (회유금속 소재 연구소) ;
  • 이상백 (순천대학교 자동차 부품 및 소재 연구 개발센타) ;
  • 김병일 (순천대학교 재료금속공학과)
  • 발행 : 2001.12.01

초록

Pure tantalum powder has been produced by sodium as a reluctant, $K_2TaF_7$as a feed material and KCl/KF as a diluent in an inconel stainless steel bomb by the metallothermic reduction. The influence of experimental variable, such as temperature of reduction on the yield and characteristics of the Ta powder has been studied. As the temperature of the reduction was varied from$ 800{\circ}C~980{\circ}C$, the yield of tantalum powder increased from 41% to 56%. However no appreciable improvement was observed above$920{\circ}C$. The fraction of fine Ta Powder decreased appreciably with the increase of temperature, and particle size was$2~3{\mu}m$at reduction temperature of$920{\circ}C$.Therefore a reduction temperature of$920{\circ}C$was optimally fixed for subsequent runs.

키워드

참고문헌

  1. G.L yudkovski, P.K. Rastogi and M. Bala, J. Met., No. 18 (1986)
  2. CIBA Limitied, Belgium Patent 625, No. 22, 178
  3. V.I. Kontantinov, S.I. Sklyarenko and E.A. Kholesbes, Poroskovaya Met. Acad. Nank SSRI, No. 4, 47 (1961)
  4. S.C. Jain, D.K. Bose and C.K. Gupta, Trans. Indian Inst. Met., No. 24, 1 (1971)
  5. K. Wayne, H. Waban and J.P. Matin, U.S Patent 2, 927, 855 (1960)
  6. Chang, U.S Patent 2, 927, 855 (1960)
  7. D.K. Bose, J.C. Sehra and P.K. Jena, Trans. Indian Inst. Met., No.23, 1 (1970)
  8. J.T. Kelly and G.A. Ress, Canadian Pat. 657, 595 (1963)
  9. Chang, U.S Patent 5, 234, 491 (1993)