Abstract
Effects of heating time and radiation under high temperature on the properties of thermal, mechanical and shielding ability of modified (KNS-101), hydrogenated bisphenol-A(KNS-201) type epoxy resin and phenol-novolac(KNS-301) type epoxy resin based neutron shielding materials that are used for shipping casks for radioactive material have been investigated. At early stages, the offset temperatures of KNS-101, KNS-201 and KNS-301 increased with the heating time under high temperature, but it was rarely affected by the heating time in the later stages. In addition, the thermal conductivities of KNS-101 and KNS-201 decreased with heating time, but that of KNS-301 increased with the heating time. On the contrary, the thermal expansion coefficients of neutron shielding materials decreased with heating time. At the high temperature, the tensile strength and flexural strength of the shielding materials decreased with heating time. On the contrary, the thermal expansion coefficients of neutron shielding materials decreased with heating time. At the high temperature, the tensile strength and flexural strength of the shielding materials of KNS-101 and KNS-301 increased with heating time, but those of KNS-201 decreased with heating time. The shielding ability of neutron shielding materials slightly increased with the radiation dose, and shielding abilities of shielding materials of KNS-101 and KNS-201 were affected to a more extent than that of KNS-301 by radiation dose under high temperature.