EFFECT OF THERMAL CYCLING AND AGING ON THE TENSILE STRENGTH OF GLASS-IONOMER RESTORATIVE MATERIALS
Thermal cycling과 시효처리가 Glass-Ionomer 수복재의 인장강도에 미치는 영향
- Baik, Byeong-Ju (Department of Pediatric Dentistry and Institute of Oral Bioscience, College of Dentistry, Chonbuk National University) ;
- Kim, Mun-Hyeon (Department of Pediatric Dentistry and Institute of Oral Bioscience, College of Dentistry, Chonbuk National University) ;
- Lee, Seung-Young (Department of Pediatric Dentistry and Institute of Oral Bioscience, College of Dentistry, Chonbuk National University) ;
- Lee, Seung-Ik (Department of Pediatric Dentistry and Institute of Oral Bioscience, College of Dentistry, Chonbuk National University) ;
-
Kim, Jae-Gon
(Department of Pediatric Dentistry and Institute of Oral Bioscience, College of Dentistry, Chonbuk National University)
- 백병주 (전북대학교 치과대학 소아치과학교실) ;
- 김문현 (전북대학교 치과대학 소아치과학교실) ;
- 이승영 (전북대학교 치과대학 소아치과학교실) ;
- 이승익 (전북대학교 치과대학 소아치과학교실) ;
-
김재곤
(전북대학교 치과대학 소아치과학교실)
- Published : 1999.11.30
Abstract
This study was performed to evaluate the effect of aging and thermal cycling on the tensile strength of six commercially available glass-ionomer materials: two chemically set glass-ionomer materials(Fuji II, Fuji IX), two resin-modified glass-ionomer materials(Fuji II LC, Vitremer), and two polyacid-modified composite resins(Compoglass, Dyract). Rectangular tension test specimens were fabricated in a teflon mold giving 5mm in gauge length and 2mm in thickness. All samples were divided into 3 groups. Group 1 was immersed in a
본 연구에서는 구강환경과 유사한 액상의 조건하에서의 온도변화가 광중합형 글래스아이오노머계 수복재의 인장강도에 미치는 영향을 평가하기 위해 대조군으로 2종의 재래형 glass ionomer를 선택하고 실험군으로 2종의 광중합형의 resin-modified glass ionomer와 2종의 polyacid-modified resin composite을 선택한 다음 수중에서의 thermal cycling과 시효처리를 행하였으며, 다음과 같은 결론을 얻었다. 1. 글래스아이오노머 수복재의 인장강도를 측정한 결과, polyacid-modified resin composite, resin-modified glass ionomer 그리고 재래형 glass ionomer 의 순으로 나타났다. 2. 인장강도는 30일간의 시효처리로 증가되는 경향을 보였다. 3. 재래형 glass ionomer 수복재의 인장강도는 thermal cycling 처리로 증가되는 경향을 보였으며,