Recovery of Mg-Ferrite Powder from Acid Leaching Mg Waste by Hydrothermal Method

산 침출 Mg폐액으로부터 수열법에 의한 Mg-Ferrite 분말회수

  • 김영순 (충남대학교 급속응고신소재연구소) ;
  • 윤기석 (충남대학교 급속응고신소재연구소) ;
  • 안찬영 (충남대학교 급속응고신소재연구소) ;
  • 이종현 (충남대학교 급속응고신소재연구소) ;
  • 원창환 (충남대학교 급속응고신소재연구소)
  • Published : 1997.12.01

Abstract

The Mg-ferrite powders were recovered from acid leaching Mg waste by hydrothermal method. Recovering conditions ofMg-Ferrite were investigated m this system and the powders prepared were characterized, using X-ray analysis, chemicalanalysis, SEM. TEM, and VSM. In this study, pH of solution and the kind of neutralizer wcre important factors on thecharacteristics of the product. The optimum condition of recovering MgPenite was the mole ratio of Fe" : Mg"=2'1, reactiontemperature : ZOWC, reaction time.lhr, at pH=lZ, and Oi partial pressure af 2000 psi. And the powders ~ccovered have amonodispersed and spherelike shapes with the narrow sue distribulion.ow sue distribulion.

본 논문은 SHS(Self propagating High-temperature Synthesis)법을 이용하여 $WO_3$/Mg 계로부터 W을 제련시 산침출로 인하여 발생하는 Mg 폐액으로부터 Mg-ferrite분말을 회수하는 방법에 대한 것으로, 습식법 주에서 단분산성 구형 초미립자들을 하소 공정없이 직접제조가능하다는 장점을 가진 수열합성법을 이용하여 Mg-ferrite분말을 회수하는 것을 중심 내용으로 하고 있다. 산침출 Mg 폐액으로부터 수열법에 의한 Mg-Ferrite 분말 회수시 폐용액의 pH와 pHwhwjf제는 분말의 특서에 크게 영향을 주었다. 분말회수의 최적조건은 ${Fe}^{2+}$ : ${Mg}^{2+}$몰비가 2:1, 반응온도가$ 200^{\circ}C$, 반응시간이 1시간, pH=12, 산소분압이 2000psi였고, 이때 제조된 분말은 단분산성, 균일한 입도분포를 가진 구형입자이었다.

Keywords