Temperature Effect On Warm Deep Drawability of Rectangular Cup Using Local Heating of Dies
금형의 국부적인 가열에 의한 사각통의 온간 디프로드로잉 성형성에 미치는 온도의 효과
- Kim, Chang-Ho ;
- Park, Dong-Hwan ;
- Kang, Sung-Soo
- 김창호 (부산대학교 기계설계공학과 대학원) ;
- 박동환 (삼성자동차(주) 부품기술팀) ;
- 강성수 (부산대학교 기계공학과, ERC for NSDM)
- Published : 1996.05.01
Abstract
Warm deep drawing of single-action dies using local heating has appeared to be an alternative attractive production method of multi-operation die sets generally used at room temperature in deep drawing of rectangular cup. Uniaxial tensile tests and deep drawing tests of various materials are carried out and the effect of temperature on tensile properties and drawability are examined at temperatures up to 200 .deg. C under three kinds of lubricants of teflon film, vinyl film and drawing oil. Good formability is achieved when punch and die temperature were differentiated intentionally in order to get large tensile strength(TS) at punch shoulder protion and small TS at die side. Throughout the experiments, it has been shown that the limiting drawing height of STS316L was increased with heating die and blank holder at 100 .deg. C, but that of STS430 wasn't. When vinyl or teflon film was attached on the plates, the drawability was increased considerably.
Keywords