A Study on the Manufacturing of Hypereutectic Al-Si Alloy Modifier by Mechanical Alloying Process and its Modification Effects

기계적합금화법에 의한 과공정 Al-Si 합금 미세화제 개발 및 개량효과에 관한 연구

  • Park, Jae-Young (Dept. of Metallurgical Engr. Seoul National University) ;
  • Lee, Jae-Sang (Dept. of Metallurgical Engr. Seoul National University) ;
  • Ra, Hyung-Yong (Dept. of Metallurgical Engr. Seoul National University)
  • 박재영 (서울대학교 금속공학과) ;
  • 이재상 (서울대학교 금속공학과) ;
  • 나형용 (서울대학교 금속공학과)
  • Published : 1995.08.20

Abstract

Recently Al-Cu-P alloys are used to refine primary Si of hypereutectic Al-Si alloys. Because it has inside AlP compound that acts as nucleation site in the melt, Al-Cu-P alloy has good refinement effect in lower holding temperature and after shoter holding times. In this study Al-Cu-P refinement agent was made by mechanical alloying method. When Al-13.5wt%Cu-1.5wt%P was alloyed mechanically for 30hr in Ar atmosphere by high energy ball mill, it had the refinement effect that showed primary Si size of about $30{\mu}m$ in Al-20wt%Si at $760^{\circ}C$, treated for 15min.

Keywords