Effect of Solid Loading and Lamination Process on the Properties of Ni-Zn Ferrite Made by Tape Casting Method

분말의 함량 및 적층공정이 Tape Casting법으로 제조된 Ni-Zn Ferrite의 물성에 미치는 영향

  • 이창호 (고려대학교 재료공학과) ;
  • 김경용 (고려대학교 재료공학과) ;
  • 이창호 (한국과학기술연구원 세라믹스연구부) ;
  • 김경용 (한국과학기술연구원 세라믹스연구부)
  • Published : 1994.06.01

Abstract

Ni0.3Zn0.7Fe2O4 ferrite specimens were fabricated by dry pressing and tape casting method. The properties of each specimen were measured and compared. In order to design and manufacture the chip devices effectively, one important criterion can be that the sintered density of the laminated body should approach close to that of the dry pressed body which is regarded as standard. This requirement could be satisfied by controlling the solid loading of the ferrite sheet, lamination temperature and pressure. Using the optimum conditions (solid loading 55 wt%, lamination temperature 6$0^{\circ}C$, lamination pressure 400 kg/$\textrm{cm}^2$, sintered at 125$0^{\circ}C$ 2h) a sintered ferrite, with the density of 5.18g/㎤ and permeability of 1390 at 0.5 MHz, were obtained.

Keywords

References

  1. Electronic Ceramics v.24 積層型 表面實製素子用, フェライト 中野敦村;野村武史
  2. Modern Ferrite Technology Alex Goldman
  3. IEEE Trans Instr Meas v.IM-19 Measurement of the Intrinsic Properties of Materials by Time Domain Techniques A.M. Nicolson(et.al)
  4. Jpn. J. Appl. Phys. v.31 no.7 Measurement Error Induced by Air Gap of Electromagnetic Wave Absorber in the Coaxial Line Method K.Y. Kim;W.S. Kim;H.J. Jung;S.D. Jang
  5. J Am Ceram. Soc. v.71 no.8 Role of Zinc Volatilization on the Microstructure Development of Managnese Zinc Ferrites P. Sainamthip;V.R.W. Amarakoon
  6. Advances in Ceramics v.15 On the Kinetics of the Vaporization of Zn Ions in the Sintering Process of Ferrites D. Condruache;C Pasincu;E. Luca
  7. J. Am. Ceram Soc v.60 no.1-2 Effects of Porosity and Grain Size on the Magnetic Properties of Ni Zn Ferrite H. Igarashi;K. Okazaki