The Extraction of Rare Earth Metal Component from the Domestic Monazite

국내부존 Monazite로부터 희토류금속의 추출

  • Hwang, Chang-Il (Dept. of Chem. Eng., College of Engineering, Dankook Univ.) ;
  • Hyun, Seong-Ho (Dept. of Chem. Eng., College of Engineering, Dankook Univ.) ;
  • Lee, Chul-Tae (Dept. of Chem. Eng., College of Engineering, Dankook Univ.)
  • 황창일 (단국대학교 공과대학 화학공학과) ;
  • 현성호 (단국대학교 공과대학 화학공학과) ;
  • 이철태 (단국대학교 공과대학 화학공학과)
  • Received : 1992.04.16
  • Accepted : 1992.05.29
  • Published : 1992.09.30

Abstract

Three type extraction processes of rare earth metal component from rare earth metal bearing ore were sulfuric acid digestion, caustic soda leaching and decomposition with $(NH_4)_2SO_4$. From the overall results, both caustic soda leaching and sulfuric acrid digestion were better extraction processes for domestic monazite ore. The proper conditions of sulfuric acid digestion for domestic monazite ore were reaction temperature $210^{\circ}C$, reaction time 40 min, weight ratio of $H_2SO_4$ to monazite ore 1.5 and concentration of $H_2SO_4$ 95%. Under these conditions, 98% of rare earth metal component was extracted and also the reasonable conditions for caustic soda leaching were reaction temperature $140^{\circ}C$, weight ratio of NaOH to monazite 3.0, concentration of caustic soda solution 50% and leaching time 3hrs. Under these conditions, 97% of rare earth metal component was extracted.

함희토류광물로부터 3가지 희토류성분의 추출공정이 국산 monazite에 대한 적절한 추출공정을 찾기위해 조사되었다. 본 연구에서 조사된 3가지 공정은 황산법, 알칼리법및 황산암모늄 분해법이었다. 실험결과로부터 황산법 및 알칼리법이 국산 monazite에 더욱 효과적인 추출공정이었음이 조사되었다. 국산 monazite에 대한 황산법의 적절한 반응조건은 반응온도 $210^{\circ}C$, 반응시간 40분, monazite에 대한 $H_2SO_4$의 고액비 1.5, 황산의 농도 95%였으며, 이 조건하에서 98%의 희토류성분이 추출되었다. 또한 알칼리법에 대한 적절한 반응조건은 반응온도 $140^{\circ}C$, monazite에 대한 NaOH의 무게비 3.0, NaOH의 농도 50%, 침출시간 3시간이었으며, 이 초건하에서 97%의 희토류성분이 추출되었다.