Abstract
Effect of Li2O.4B2O3 frit addition on microstructural and thermal expansion behaviour of the $\beta$-spodumene ceramics made from kaolinite was investigated. With 2.0~4.0 wt% frit addition, the densification by liquid phase sintering caused low water absorption below 3% and enhancement of beding strength. As the amount of frit addition was increased, thermal expansion coefficient was increased to large scale, but in 2 wt% frit addition, its thermal expansion coefficient was constrained to 1.92$\times$10-6$^{\circ}C$-1.