Separation and Utilization of Main Components of Hardwood by Organosolv Pupling

Organosolv 방법(方法)에 의(依)한 활엽수(闊葉樹) 주요(主要) 조성분(組成分)의 분리(分離) 및 이용(利用)

  • 투고 : 1988.11.05
  • 발행 : 1988.12.30

초록

To separate and utilize the main components of hardwood (Quercus mongolica) by organosov pulping (ester pulping), chips were cooked at various conditions such as; the solvent ratio (acetic acid: ethylacetate: water, 50:25:25; 33:33:34; 25:50:25), maximum temperature (165, 170, $175^{\circ}C$), and cooking times (2, 2.5, 3 hr). The pulps were bleached by the sequences of CEDED, C/DEDED, PEDED. Lignin, sugars, and acetic acid were separated from black liquor and washing liquors. 1. The selective delignification at optimal pulp yield (43-45%) was obtained by cooking at acetic acid: ethylace tate: water ratio of 33:34:34 for 3 hr at $170^{\circ}C$. But in this case, kappa no. of the pulp was not reduced under 60 points. 2. Kappa no. of the pulp could be dropped by an acetone wash to remove reprecipitated lignin a t cooked pulp. 3. The unbleached pulps had a brightness of 45-50%, whereas the bleached pulps gave at 88-93% brightness. Tensile, burst, and tear strengths of the bleached pulps were lower than those of kraft pulp, especially in tear strength. The pulps which were bleached with CEDED sequence were higher in strengths than another bleaching sequences. 4. Lignin of 90-95%(lignin base on wood)was separated from black liquor and washing liquors, while the purified sugars and recovery of acetic acid were a low. An organic phase composed of acetic acid, ethylacetate, and water was separated to a two-phase system by proper adjustment of the solvent ratios.

키워드