Abstract
The water gas shift conversion catalyst prepared by the American Cyanamide Co. was subjected to fluidization in a 2-in. Pyrex glass tube to obtain the basic fluidization characteristic data. The size of the catalyst charged ranged from 70 to 120 meshes and it was supported on a single layer 300-mesh wire gauze through which the fluidizing medium, the air, was passed. Following are some data and facts found by the authors: (1) The catalyst particles were porous, and their surfaces were trough and irregular. (2) The average effective particle density and the average shape factor of these particles were 152.2 lb/$ft^3$ and 0.865 respectively. (3) As the particle diameter of the catalyst increased, the minimum fluid voidage of the bed decreased slightly. (4) Just before the incipient fluidization, pressure drop suddenly fell and the bed expanded simultaneously. (5) After fluidization set in, the expansion characteristics of the catalyst bed were similar to those of sand and glass beads except intense bubbling in the catalyst bed.