13mm 크기 순환굵은골재 치환이 콘크리트의 공학적 특성에 미치는 영향

Effect of Replacement of Recycled Coarse Aggregate with 13mm on Engineering Properties of the Concrete

  • 발행 : 2014.11.14

초록

The aim of this research is suggesting the method of obtaining well-graded aggregates for concrete replacing the recycled aggregate which size range is from 5 to 13 mm to currently used gap-graded natural aggregates which size range is only 13 to 25 mm. according to the tests results, the workability of concrete was improved with replacing the aggregates of 5 to 13 mm of size range because of compensating gap-grading. Furthermore, there was an improvement in compressive strength when the aggregates of 5 to 13 mm of size range was replaced because obtained well-graded aggregates contributed on increasing adhesiveness and filling internal pore system. Comparing replacing recycled aggregate to natural aggregate, there was no significant difference on the performances.