Proceedings of the Materials Research Society of Korea Conference (한국재료학회:학술대회논문집)
- 2009.05a
- /
- Pages.44.2-44.2
- /
- 2009
Materal properties of Porous BCP Scaffolds depending on the process conditions
Abstract
BCP powder was synthesized using microwave hydrothermal process with mixed calcium hydroxide and phosphoric acid. After using replica method, porous BCP scaffold was fabricated. PU (Poly Urethane) was used as the fugitive skeleton to fabricate the porous scaffold. BCP powder was mixed in PVB (Polyvinyl butyral) and ethanol solution and then applied to the PU foam by dip coating. After several times of coating and the subsequent oven drying the coated PU foam was burnt out at