Reduction of hexavalent chromium (Cr(VI)) under acidic conditions during its determination in cement

시멘트 6가 크롬 (Cr(VI))정량분석법에 관한 고찰 - 분석과정에서 Cr(VI) 의 환원에 따른 오차제어-

  • 문세흠 (삼성건설기술연구소, 기반기술연구팀) ;
  • 정재홍 (삼성건설기술연구소, 기반기술연구팀) ;
  • 이승훈 (삼성건설기술연구소, 기반기술연구팀) ;
  • 이승헌 (군산대학교, 신소재.나노화학공학부)
  • Published : 2008.04.24

Abstract

Some substances of cement could make underestimate concentration of hexavalent chromium(Cr(VI)) as they reduce Cr(VI) to Cr(III) in acidic condition during the determination of Cr(VI) content in cement. The reduction of Cr(VI) increased with elapsed time after acidification in this study. The reduction rate varied with various cements. From our result, we can conclude that simultaneous additions of acid and DPC were required for the accurate measurement of Cr(VI) in cement. The high recovery rate of 94.3 to 106.7% with the simultaneous acid-DPC addition method can also support our conclusion.

시멘트내 6가 크롬의 분석은, 산성조건에서 6가 크롬이 디페닐카르바지드(DPC)와 결합하여 적자색의 착화합물을 형성하는 것을 원리로 한다. 그러나 6가 크롬은 산성조건에서 강한 산화력을 가지고 있기 때문에 철, 황화물, 유기물 등이 존재하는 경우 해당물질을 산화시키고 3가로 환원된다. 시멘트에는철, 황화물 등의 다양한 환원물질이 존재하기 때문에 분석과정에서 6가 크롬이 과소측정될 가능성이있다. 본 논문에서는 최근 제정된 "시멘트 중 6가 크롬의 정량분석 방법 (KS L 5221)"의 근간이 되는 JCAS I-51 실험방법 중 황산첨가 후 DPC 첨가의 경과시간에 따른 6가 크롬의 실험오차에 대해 검증하였다. 실험결과 황산첨가 후 시간이 경과함에 따라 측정되는 6가 크롬의 농도가 감소하였으며 감소효과는 시멘트마다 다르게 나타내었다. 인위적으로 용출액에 크롬을 첨가한 후 회수율을 측정한 결과, 산-DPC를 동시에 투입한 경우 $94.3{\sim}106.7$%의 회수율을 나타내었다.

Keywords