Evaluation of Microstructural and Mechanical Properties of SA508 cl.3 Heat Affected Zone Produced by RPV Cladding

  • Lee, J.S. (Center for Advanced Reactor Research, KAIST) ;
  • Kim, I.S. (Department of Nuclear and Quantum Engineering, KAIST) ;
  • Kwon, S.C. (Korea Atomic Energy Research Institute)
  • Published : 2004.10.28

Abstract

The maximum width of HAZ of SA508치.3 steel produced by overlay RPV cladding was approximately 10 mm and it was composed of variety of microstructures with various grain size and precipitates. In addition, along the weld fusion line there formed a heavy carbide precipitation zone in the width of $20{\sim}30\;{\mu}m$. 2. As the specimen sampling position approached to the weld fusion line, the increase in yield and tensile strength was approximately 90 and 40 MPa, respectively. Meanwhile, the plastic fracture strain reduced from 14 to 8 percent. 3. The lowest SP energy and the highest ductile to brittle transition temperature in the HAZ were observed at the coarse- and fine-grained HAZ.