$CaCO_3$ 첨가에 따른 저온소결 PNW-PMN-PZT 세라믹스의 압전 및 유전 특성

Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PNW-PMN-PZT Ceramics with the Amount of $CaCO_3$ Addition

  • 발행 : 2004.11.11

초록

In this study, in order to develop low temperature sintering ceramics for ultrasonic vibrator, PNW-PMN-PZT system ceramics were manufactured with the amount of $CaCO_3$ addition and their piezoelectric, dielectric and microstructural characteristics were investigated. $CaCO_3$ addition to PNW-PMN-PZT basic composition was proved to be capable of sintering the ceramics at temperature below $1000^{\circ}C$ due to the effect of $Li_2CO_3-CaCO_3$ liquid phase. However, with increasing the amount of $CaCO_3$ addition, the second phase was appeared. As the results, electromechanical coupling coefficient (kp) and dielectric constant $(\epsilon_r)$ decreased. Taking into consideration electromechanical coupling coefficient (kp) of 0.49, mechanical quality factor (Qm) of 1396, dielectric constant $(\epsilon_r)$ of 1300 and density of $7.78[g/cm^2]$, it was concluded that the 0.25wt% $CaCO_3$ addition composition ceramics sintered at $920^{\circ}C$ was suitable for ultrasonic vibrator application.

키워드