Abstract

IAEA, FT-04-020, and ANS 16.1, standard leaching test methods, were evaluated comparatively with their test results. Leaching index of Co-60 and Cs-137 for all waste forms were above 6.0. Their leaching behavior were contrary according to the type of matrix and leachant. Leachability of Co in cement waste form was higher in simulated seawater than demi. water, and higher in demi. water in paraffin waste form. Leachability of Cs was contrary to Cs. Cumulative fraction leached of Co was higher such as IAEA>ANS>FT in cement waste form.

IAEA, FT-04-020, ANS 16.1의 침출시험법을 각각 수행하여 얻은 시험결과를 이용하여 상호비교 평가하였다. 붕산을 함유한 파라핀 및 시멘트 고화체에서의 Co-60과 Cs-137의 침출지수는 6이상이었으나 고화매질과 탈염수의 종류에 따라 상반되는 침출거동을 보였다. 침출수로 합성해수와 탈염수를 사용하였을 경우 Co는 시멘트 고화체에서는 합성해수, 파라핀 고화체에서는 탈염수에서 침출이 높았다. 반면에 Cs의 침출정도는 시멘트에서는 탈염수, 파라핀에서는 합성해수에서 높았다. Co의 침출분율은 시멘트 고화체에서 IAEA > ANS > FT의 순으로 높았으며, 반대로 파라핀 고화체에서는 이의 역순이었다.

Keywords