초록
$(Ba_{0.6-x}Sr_{0.4}Ca_x)TiO_3$(BSCT) (x=0.10, 0.15, 0.20) powders were prepared by the sol-gel method and BSCT thick films were fabricated by the screen-printing method. The structural properties as a faction of the composition ratio were studied. As a result of the differential thermal analysis (DTA), exothermic perk was observed at around $860^{\circ}C$ dne to the formation of the polycrystalline perovskite phase. The BSCT thick films sintered at $1350^{\circ}C$ for 2h showed the average grain size of $2{\sim}7{\mu}m$. The average thickness of BSCT thick films, obtained by 3 times of screen-printing, was approximately $85{\mu}m$.