후속 열처리 온도에 따른 SBT 커패시터의 전기적 특성

Electrical Properties SBT capacitor with post-annealing

  • 발행 : 2001.07.01

초록

The Sr$\sub$0.8/Bi$\sub$2.4/Ta$_2$O$\sub$9/(SBT) thin films are deposited on Pt-coated electrode(Pt/TiO$_2$/SiO$_2$/Si) using RF magnetron sputtering method. With increasing annealing tempera ture from 600[$^{\circ}C$] to 850[$^{\circ}C$], Bi-layered perovskite phase was crystallized above 650[$^{\circ}C$]. The maximum remanent polarization and the coercive electric field is 11.60[${\mu}$C/$\textrm{cm}^2$], 48[kV/cm] respectively. The dielectric constant and leakage current density is 213, 1.01${\times}$10$\^$-8/ A/$\textrm{cm}^2$ respectively at annealing temperature of 750[$^{\circ}C$].