The tungsten disulfide (WS$_2$) solid lubricant was synthesized by two different reaction processes, and the chemical and physical characteristics of synthesized WS$_2$ powder were analyzed in terms of the average particle size, morphology, crystalline phase. The solid WO$_3$ powder with the average size of 0.2 $\mu$m was reacted with CS$_2$ gas flowed with N$_2$ or 96% N$_2$ + 4% H$_2$ forming gas for 36 h and 24 h at 900$\circ$C respectively. In the case of vapour phase transport method, the 3.5 wt% iodine was added as a vapour transport reagent into the composition of tungsten and sulfur powders maintaining a constant molar ratio of W : S = 1 : 2.2. The mixture was then heat treated at 850$\circ$C for 2 weeks in vacuum The reaction product obtained showed the average size of 12 $\mu$m and the hexagonal plate shape of typical solid lubricant with 2H-WS$_2$ crystalline phase.

Keywords